Temafloor 200 Primer

Coatings
DESCRIPTION A two component solvent free epoxy varnish.
PRODUCT FEATURES For impregnating and priming of new and old concrete floors prior to laying Temafloor coatings and screeds. Thinned Temafloor 200 penetrates well into the pores of the concrete sealing the surface and giving good adhesion for coatings and screeds. Mixed with sand also suitable for patching of concrete floors.
RECOMMENDED USES Concrete floors.

TECHNICAL DATA
Gloss groups Full-gloss
Coverage

Coverage on concrete floors is on the average:

1st primer coat                     4 - 8 m2/l

2nd primer coat                  6 - 10 m2/l

 

Practical coverage depends on the porosity and evenness of the substrate and on the application method.
Thinner 1029 and 1031
Mixing ratio Base 2 parts by volume 008 4400
Hardener 1 part by volume 930 5145
Application method Roller, steel or rubber trowel.
Pot-life (+23°C) About 15 minutes after mixing, on substrate.
Drying time at 23°C and 50% relative air humidity

Dust dry after 3 hours

Touch dry after 5 hours

Recoatable after 6 - 12 hours

Light trucking after 16 hours

Fully cured after 7 days

 

The drying times are for Temafloor 200 Primer thinned 30 % with Thinner 1029.
Solids volume Approx. 100 volume %
Density 1.1 kg / litre (mixture)
Product code 008 4400

APPLICATION DETAILS
Application conditions The relative humidity of the concrete should not exceed 97 %. The temperature of the ambient air, surface or coating should not fall below + 15 ºC during application or drying. Relative humidity of air should not exceed 80 %.
Preparation New concrete: Remove laitance by power grinding, vacuum grit blasting or hydrochloric acid etching. Choose the method best suited for the premises. After grinding remove dust carefully with a vacuum cleaner. Hydrochloric acid etching is carried out with diluted hydrochloric acid (1 part concentrated hydrochloric acid, 4 parts water). Rinse with plenty of water. Dry the floor.

Old concrete: Remove all grease, oil, chemicals and other impurities by MAALIPESU detergent. Remove old peeling paint layer by grinding or vacuum grit blasting. Clean out pot-holes removing all loose friable material. Open cracks with e.g. an abrasive tool. Remove loose material and dust.
Priming Prime using 30 - 50% thinned Temafloor 200 Primer epoxy varnish. Pour the varnish onto the floor and apply as much as is needed to impregnate the concrete surface. If necessary, repeat priming to get a non-porous surface. Subsequent treatment can be carried out after 2 hours using "wet-on-wet" technique.
Patching Patch pot-holes and cracks with a mixture of unthinned Temafloor 200 Primer epoxy varnish and dry, clean sand. Mixing ratio e.g. 1 part by volume of varnish mixture and 1 - 2 parts by volume of sand of grain size 0.1 - 0.6 mm. If the topcoat will be applied as a thin layer, grind the patched areas before overcoating.
Coating Overcoating may be carried out 6 - 12 hrs after priming. If the primed surface is not overcoated within 24 hrs, it should be abraded. A porous primer coat will result in holes and air bubbles in the finished coating.
Mixing of components Mix the correct proportions of base and hardener thoroughly (approx. 2 minutes) by using an industrial hand drill with a paddle. The amount of mixture depends on the area to be coated and on the pot life of the mixture. Insufficient mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the coating and risk the success of the application.
Cleaning of tools Thinner 1029 (or Thinner 1031).
EU VOC 2004/42/EC-limit value VOC 2004/42/EC (cat A/j) 500 g/l (2010)
Temafloor 200 Primer: max. VOC < 500 g/l

HEALTH AND SAFETY CLASSIFICATION
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj.
Product safety data sheetTEMAFLOOR 200 EPOXY VARNISH [GB-ENG]
Thinner safety data sheetTHINNER 006 1029 [GB-ENG]
Hardener safety data sheetTEMAFLOOR 200, 3000 SL, P300 and 150 HARDENER [GB-ENG]
 
-

CE
The European harmonized productstandard EN 13813 defines the requirements for Screed materials and floor screeds, including synthetic resin screeds.

This product is tested and CE-labelled in accordance with the tables ZA.1.5 and ZA.3.3 in the appendix ZA.3.
CE logo
Tikkurila Oyj
P.O.Box 53
FI-01301
Vantaa
11
EN 13813 SR-B2,0
Primer
Reaction to fire E 1)
Release of corrosive substances SR
Water permeability NPD
Abrasion resistance NPD
Bond strength B2,0
Impact resistance NPD
Sound insulation NPD
Sound absorption NPD
Thermal resistance NPD
Chemical resistance NPD
1) In accordance with the Commission decision 2010/85/EC

The above information, based on laboratory tests and practical experience, has been proved valid at the date marked on the product data sheet. The quality of the product is ensured by our operational system, based on the requirements of ISO 9001 and ISO 14001. As a manufacturer we cannot be responsible for any damages caused by using the product against our instructions or for inappropriate purposes.