PRODUCT DATA SHEET 18.02.2010 |
|||||||||||||||||||||
Temabond ST 300 |
|
|||||||||||||||||||||
| DESCRIPTION | A two component high-solids, modified epoxy paint. | |||||||||||||||||||||
| PRODUCT FEATURES | Especially used as a primer for steel surfaces difficult to clean in process and chemical industry and in water immersion. Recommended for repairing of damages caused by transport or installation. Can also be applied on old alkyd paint surfaces. Can be used as a single coat paint. | |||||||||||||||||||||
| RECOMMENDED USES | Steel surfaces. | |||||||||||||||||||||
| TECHNICAL DATA | ||||||||||||||||||||||
| Features | Forms a tight coat with good chemical and abrasion resistance. High film build properties, also by brush. Very good adhesion to blast cleaned or hand prepared steel. Low solvent content, lower solvent emissions than with traditional epoxy paints. | |||||||||||||||||||||
| Colour Range | TEMASPEED tinting. | |||||||||||||||||||||
| Gloss groups | Gloss | |||||||||||||||||||||
| Coverage |
Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated. |
|||||||||||||||||||||
| Thinner | 1031 | |||||||||||||||||||||
| Mixing ratio | Base 1 part by volume 162-series
Hardener 1 part by volume 008 7501 |
|||||||||||||||||||||
| Application method | By airless spray or brush. | |||||||||||||||||||||
| Pot-life (+23°C) | 1½ hours | |||||||||||||||||||||
| Drying times |
Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation. |
|||||||||||||||||||||
| Solids volume | 80 ± 2 voulume % (ISO 3233)
88 ± 2 weight % |
|||||||||||||||||||||
| Density | 1.5 kg / l (mixed) | |||||||||||||||||||||
| Product code | 162-series | |||||||||||||||||||||
| APPLICATION DETAILS | ||||||||||||||||||||||
| Application conditions | All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below +10 ºC during application and drying. Relative humidity should not exceed 80 %. The surface temperature of the steel should remain at least 3 ºC above the dew point. | |||||||||||||||||||||
| Preparation | Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)
Steel surfaces: Remove rust by tool cleaning to minimum St2 or blast clean to Sa2 or Sa2½. Blast clean to grade Sa2½ for immersion. (ISO 8501-1) Earlier painted surfaces: Roughen old paint surfaces using e.g. abrasive wheel, sand paper or blast cleaning. |
|||||||||||||||||||||
| Priming | Temabond ST 200, Temabond ST 300, Temazinc 77, Temazinc 99 and Fontecoat EP Primer. | |||||||||||||||||||||
| Finishing | Temacoat GPL, Temacoat GPL-S MIO, Temacoat GPL-S Primer, Temacoat GS 50, Temacoat RM 40, Temacoat HS 40, Temabond ST 300, Temadur, Temathane and Temacryl EA. | |||||||||||||||||||||
| Painting | By airless spray or brush. Depending on the temperature of the components the paint can be thinned 0 - 10 %. Airless spray nozzle tip 0.013" - 0.019" and nozzle pressure 120 - 180 bar. Spray angle shall be chosen according to the shape of the object. At brush application the paint should be thinned according to the circumstancies. | |||||||||||||||||||||
| Mixing of components | First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing. | |||||||||||||||||||||
| Cleaning of tools | Thinner 1031. | |||||||||||||||||||||
| EU VOC 2004/42/EC-limit value | The Volatile Organic Compounds amount is 195 g/litre of paint mixture.
VOC content of the paint mixture (thinned 10 % by volume) is 260 g/l. Only for industrial and professional use. |
|||||||||||||||||||||
| HEALTH AND SAFETY CLASSIFICATION | ||||||||||||||||||||||
| Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj. | ||||||||||||||||||||||
| Product safety data sheet | TEMABOND ST 300 [GB-ENG] | |||||||||||||||||||||
| Thinner safety data sheet | THINNER 1031 [GB-ENG] | |||||||||||||||||||||
| Hardener safety data sheet | TEMABOND ST 200 and ST 300 HARDENER [GB-ENG] | |||||||||||||||||||||
| - | ||||||||||||||||||||||
The above information, based on laboratory tests and practical experience, has been proved valid at the date marked on the product data sheet. The quality of the product is ensured by our operational system, based on the requirements of ISO 9001 and ISO 14001. As a manufacturer we cannot be responsible for any damages caused by using the product against our instructions or for inappropriate purposes.