Temaprime GF

DESCRIPTION A fast drying, one component anti-corrosive pigmented special primer.
PRODUCT FEATURES Primer for steel, aluminium and zinc surfaces. Recoatable also with polyurethane paints. Can also be used without any topcoat for steel surfaces in dry indoor areas.
RECOMMENDED USES Recommended uses e.g. haulage equipment, agricultural, construction and other machinery.

TECHNICAL DATA
Features Excellent anti-corrosive properties.
Colour Range Grey (TVT 4001). TEMASPEED tinting.
Gloss groups Matt
Coverage

Recommended film thicknesses

Theoretical coverage

dry

wet

 

40 µm

80 µm

12.5 m2/l

60 µm

120 µm

8.3 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Thinner 1006 and 1053
Application method By airless spray or by brush.
Drying times

DFT 50 µm

+ 10 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

50 min

15 min

10 min

Touch dry, after

2 h

1 h

30 min

Recoatable, min. after

2 h

1 h

30 min


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Solids volume 50 ± 2 % volume (ISO 3233)
68 ± 2 % weight
Density 1.3 kg / l
Product code 187-series

APPLICATION DETAILS
Application conditions All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below 5ºC during application and drying. The relative humidity should not exceed 80%. The temperature of the substrate should remain at least 3ºC above the dew point.
Preparation Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.

Zinc surfaces: Sweep blast clean with mineral abrasives, e.g. quartz sand, to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with PANSSARIPESU detergent.

Hot dip galvanized surfaces are recommended to be painted with a mist coat (paint thinned 25 - 30%) before the actual priming.

Aluminium surfaces: Sweep blast clean with non-metallic abrasives to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with MAALIPESU detergent.

Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Priming Temaprime GF.
Finishing Temalac, Temadur, Temathane, Temacryl EA, Fontecryl and Fontelac.
Painting By airless spray or by brush. Mix the paint thoroughly before use. The paint can be thinned 0 - 15% at airless spray application. Airless spray nozzle tip 0.011" - 0.013" and nozzle pressure 120 - 180 bar. Spray angle shall be chosen according to the shape of the object. Large surfaces Thinner 1053 (slow).
Cleaning of tools Thinner 1006.
EU VOC 2004/42/EC-limit value The Volatile Organic Compounds amount to 440 g/litre of paint.
VOC content of the paint (thinned 15 % by volume) is 500 g/l.
Only for industrial and professional use.

HEALTH AND SAFETY CLASSIFICATION
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj.
Product safety data sheetTEMAPRIME GF [GB-ENG]
Thinner safety data sheetTHINNER 1006 [GB-ENG]
-

The above information, based on laboratory tests and practical experience, has been proved valid at the date marked on the product data sheet. The quality of the product is ensured by our operational system, based on the requirements of ISO 9001 and ISO 14001. As a manufacturer we cannot be responsible for any damages caused by using the product against our instructions or for inappropriate purposes.