PRODUCT DATA SHEET
08.02.2010

Temasolid SC-F 80 - Polyurea paint

 
Temasolid SC-F 80
DESCRIPTION A two component gloss polyurea paint, containing anticorrosive pigments, hardener aliphatic isocyanate.
PRODUCT FEATURES

Recommended to be used especially as a single coat finish for agricultural and earth moving machinery and other machinery and equipment. Excellent weathering and abrasion resistance. A durable, easy to clean and non-chalking paint with exellent gloss and colour retention.

Recommended uses Agricultural and earth moving machinery and other machinery and equipment.

TECHNICAL DATA
Colour Cards RAL, NCS, SSG, BS, MONICOLOR NOVA, SYMPHONY, TEMASPEED Tinting
Gloss groups Gloss
Coverage

Recommended film thicknesses

Theoretical coverage

dry

wet

 

  80 µm

100 µm

10.0 m2/l

120 µm

150 µm

6.7 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Thinner 1048 and 1067
Mixing ratio Base 2 parts by volume 578-s
Hardener 1 part by volume 008 7710
Application method

By airless or conventional spray.

Pot-life (+23°C) ½ hour.
Drying times

DFT 80 µm

+23 ºC / RH 30 %

+ 23 ºC / RH 50 %

+23°C /  RH 80 %

Dust dry, after

50 min

25 min

25 min

Touch dry, after

2 h

1h 15 min

35 min


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Solids volume 80 ± 2 %.
87 ± 2 %.
Density 1.4 ± 0.1 kg / l (mixed).
Product code 578-s

APPLICATION DETAILS
Application conditions All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below +5ºC during application or drying. The surface temperature of the steel should remain at least 3ºC above the dew point.
Preparation Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)
Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is necessary for cold rolled steel to improve adhesion.
Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Priming Fontecryl AP, Fontecoat EP Primer, Temanyl PVB, Temadur HS Primer,Temacoat GPL-S Primer, Temacoat SPA Primer, Temazinc 77/88/99.
Finishing Temasolid.
Painting By airless or conventional spray.
Airless spray: depending on the temperature of the components and shape of the object the paint can be thinned 0 - 10 %. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 160 - 200 bar. Spray angle shall be chosen according to the shape of the object.
At conventional spray the paint should be thinned 5 - 15 %, nozzle pressure 2,5 bar, nozzle tip 1,6-1,8 mm.
Mixing of components First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
Cleaning of tools Thinner 006 1048 or Thinner 006 1067.
EU VOC 2004/42/EC-limit value The Volatile Organic Compounds amount is 170 g/litre of paint mixture.
VOC content of the paint mixture (thinned 15 % by volume) is 270 g/l.

HEALTH AND SAFETY LABELLING
according to Regulation (EC) No. 1272/2008
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oy.
Safety data sheetTemasolid SC-F 80
Thinner safety data sheetTemasolid SC-F 80
Hardener safety data sheetTemasolid SC-F 80
 
-


Back