Working instructions
Product data sheet
Paint calculator
Safety Data Sheets

Temafloor AC 602 Clear

A two-component, solvent-free acrylic topcoat.
A non-yellowing top lacquer for Temafloor AC 502 acrylic troweling screed.

Quick and cost-effective product

Due to its hardening mechanism, the floor dries quickly and can be loaded as soon as two hours after coating. Thanks to their drying speed, the Temafloor AC coating systems are particularly suitable for
premises where the available working time is limited, such as at industrial production facilities. All Temafloor AC products can be applied in low temperatures.

Temafloor AC - floor acrylic coating system for frost and weather exposure

The Temafloor AC frost- and weatherresistant floor coating system provides many significant benefits: forms an elastic protective surface that is impact-resistant and fills in cracks, suitable for cold conditions and excellent resistance to sunlight and extreme temperature variations.


Temafloor AC 602 Clear is mainly used for:


Temafloor AC602 Clear - Solvent-free acrylic topcoat

Temafloor AC602 Clear
DESCRIPTION A two-component, solvent-free acrylic topcoat.
PRODUCT FEATURES Recommended for the floors of engineering workshops, warehouses, cold stores of food industry, parking deck surfaces, loading ramps and terraces.
Recommended uses Used as a topcoat for Temafloor AC502 acrylic troweling screed.

Features Forms elastic and durable surface.
Cures at low temperatures.
Gloss groups Semi-matt

Coverage is on the average:


Topcoat: 1.3–2.5 m2/l


Practical coverage depends on the porosity and evenness of the surface and on the application method.
Can sizes 200 l drum, content 190 kg.
Application method Topcoat Temafloor AC602 Clear lacquer mixture is applied with a rubber trowel and level with a roller.
Special feature Mixing table

Temperature (oC)*

The amount of hardener (percentage of weight of the binder)

Pot life (min)

Drying time (min)



ab. 40

ab. 70



ab. 35

ab. 75



ab. 15

ab. 35



ab. 25

ab. 70

* Temperature of the binder, air and the floor.

Possible hardeners: BP-50-FT, Perkadox®CH-50 or PEROXAN BP-Pulver 50 W.
Solids volume approx. 100 vol-%.
Density 0.95 kg /l (ready made mixture)
Product code 001 6091

Application conditions The relative humidity of the concrete should not exceed 97%. The temperature of the ambient air, surface or coating should not fall below +5ºC during either application or drying. Relative humidity of air should not exceed 80%.
Preparation New concrete
Remove laitance by power grinding, vacuum grit blasting or hydrochloric acid etching. Choose the method best suited for the premises. After grinding remove dust carefully with a vacuum cleaner. Hydrochloric acid etching is carried out with diluted hydrochloric acid (1 part concentrated hydrochloric acid, 4 parts water). Rinse with plenty of water. Dry the floor.

Old concrete
Remove all grease, oil, chemicals and other impurities by MAALIPESU detergent. Remove old peeling paint layer by grinding, milling or vacuum grit blasting. Choose the method best suited for the premises. Clean out pot-holes removing all loose friable material. Open cracks with e.g. an abrasive tool. Remove loose material and dust.
Diluting Do not thin.
Lacquering Topcoating can be carried out after the coating or screed has cured. Pour the varnish mixture onto the floor, spread with a rubber trowel and level with a roller.
Observe a right amount of hardener. Using excessive amounts of hardener can cause yellowing and may weaken the properties of the topcoat. The film thickness of the Temafloor AC602 should be 0,4–0,8 mm. Too thick film thickness may also cause yellowing of the surface.
Mixing of components Mix the correct proportions of base and hardener powder thoroughly (approx. 2 minutes) by using a hand drill with a paddle, concrete mixer or power mixer. The amount of mixture depends on the area to be coated and on the pot life of the mixture. Insufficiejnt mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the varnish and risk the success of the application.
Cleaning of tools Cleaning of equipment with Thinner 006 1400.
EU VOC 2004/42/EC-limit value VOC 2004/42/EC (cat A/j), 500 g/l (2010)
Temafloor AC602 Clear: max. VOC < 500 g/l

according to Regulation (EC) No. 1272/2008
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj. For professional use only.
Safety data sheetTEMAFLOOR AC602 CLEAR [GB-ENG]